The Optimization Tests of Robiniapseudoacacia/ Wastepaper Composite Particle Board

Fang DING, Qiuhui ZHANG, Zhigao LIU

Abstract


This article research that how the single-factor variable affect the MOR and thickness swelling rate of the particle board via orthogonal experiments. The optimum condition of the maximum MOR value is 20% resin content, 120℃ hot pressing temperatures, 10 minutes hot pressing time and the proportion of Robiniapseudoacacia/ wastepaper(w/w) is 1/1. Under this situation the MOR of composite particle board is 15.4MPa and the thickness swelling rate is 16.37%. The order of the factors from majority to minority influence is resin content > proportion of Robiniapseudoacacia/ wastepaper (w/w) > hot pressing time> hot pressing temperatures.
Key words: Robiniapseudoacacia; Wastepaper; Orthogonal Experiments; MOR

References


China Paper Association. (2007). The annual report of China's paper industry in 2006, China Pulp & Paper Industry, 28 (6), 5-15.

SONG, HU.(2005). Research on Hornification of Recycled Fiber, South West Pulp and Paper, 34(4), 28-31

SHAO Suying, HU Kaitang. (2002). Hornification of Recycled Fiber, China Pulp and Paper, 2, 57-60


Full Text: PDF

Refbacks

  • There are currently no refbacks.


Reminder


We only use three mailboxes as follows to deal with issues about paper acceptance, payment and submission of electronic versions of our journals to databases:
caooc@hotmail.com
ans@cscanada.net;ans@cscanada.org